C2.5-4-3.8 Laminated Flux Concentrator
Magnetic Characteristics
| Parameter | Material | Typical Value | Unit |
|---|---|---|---|
| Relative Permeability | Ni-Fe | 100'000 | a.u. |
| Si-Fe | 40'000 | ||
| Initial Relative Permeability | Ni-Fe | 7000 | a.u. |
| Si-Fe | 2500 | ||
| Saturation Flux Density | Ni-Fe | 1 | T |
| Si-Fe | 1.5 | ||
| Hysteresis | Ni-Fe | 2.8 | A/m |
| Si-Fe | n/a | ||
| Curie Temperature | Ni-Fe | 450 | °C |
| Si-Fe | 700 |
Material Specification
| Material Specification | Lamination | Ni or Si content |
|---|---|---|
| Lamination and Nickel content | 0.35mm | 48% (Ni) |
| Lamination and Silicon content | 0.35mm | <3.5% (Si) |
Geometry C2.5-4-3.8 (*)
| Order code | A=Air Gap | B=Wall Thickness | C = External Length | D = External Width | E = Internal Length | F = Internal Width | G = Thickness | Material |
|---|---|---|---|---|---|---|---|---|
| C-2.5-4-3.8-NiFe | 2.5 | 4 | 14 | 14 | 6 | 6 | 3.8 | Ni-Fe |
| C-2.5-4-3.8-SiFe | 2.5 | 4 | 14 | 14 | 6 | 6 | 3.8 | Si-Fe |